How to dehydrate LiTFSI?
Jun 9,2026
LiTFSI is highly hygroscopic. To dehydrate it you need to dry it in a vacuum oven at 80 °C to 140 °C for a minimum of 12 hours. This process is necessary if you use LiTFSI for battery applications.