武汉海山科技有限公司
首页 产品目录 产品目录(简版) 公司动态 企业认证 公司相册 联系我们

26.03%!多位点小分子“螯合”Li⁺,让n-i-p钙钛矿更高效、更稳定

发布人:武汉海山科技有限公司

发布日期:2026/11/18 9:54:59

26.03%!多位点小分子“螯合”Li⁺,让n-i-p钙钛矿更高效、更稳定


Li-TFSI掺杂的Spiro-OMeTAD是高效n-i-p钙钛矿太阳能电池的“标杆”空穴传输层,但Li⁺迁移长期被视为高性能与高稳定性之间的难解矛盾。近日,河北师范大学、大连理工大学、云南师范大学等合作团队在 Advanced Science 发表研究,提出多位点小分子螯合策略:设计D-A-D型分子TPABT1/2/3,利用苯并噻二唑N原子和甲氧基O原子协同配位Li⁺,在保留Li-TFSI掺杂能力的同时“锁住”Li⁺。基于TPABT3的n-i-p FAPbI₃器件获得26.03%冠军效率,未封装器件在ISOS-L-1条件下MPP跟踪1000 h后仍保持90%以上初始效率。


1.0.png


Doping mechanism of control and TPABT-doped Spiro-OMeTAD HTLs. (a) Schematic illustration of the mechanism in the conventional doping process (Spiro-OMeTAD HTLs doped with Li-TFSI). (b) Schematic illustration of the mechanisms of Li+ migration suppression and p-doping promotion via TPABT-doped Spiro-OMeTAD HTLs.

 

亮点速览

不换Li⁺,而是“ immobilize”Li⁺:保留Li-TFSI的p型掺杂能力,同时抑制Li⁺迁移和聚集。多配位位点设计:TPABT分子同时含N给体和甲氧基O给体,TPABT3引入更多–OMe,Li⁺结合更强。一石多效:抑制Li⁺迁移、促进Spiro-OMeTAD氧化、改善分子有序堆积、优化能级对齐。效率26.03%:两步法FAPbI₃ n-i-p器件,JSC 26.39 mA cm⁻²、VOC 1.17 V、FF 84.08%。稳定性提升:未封装器件ISOS-L-1 MPP跟踪1000 h保持>90%初始PCE。

 

Li-TFSI掺杂Spiro-OMeTAD的“老问题”

Spiro-OMeTAD需要Li-TFSI实现足够电导率和空穴迁移率,t-BP则用于改善Li-TFSI溶解性与成膜均匀性。但传统掺杂体系存在固有隐患:在工作条件下,小尺寸Li⁺易在器件堆叠中扩散,引发电极/界面退化与钙钛矿晶格畸变;Spiro-OMeTAD的环境氧化缓慢导致重复性差;高温下还可能形成针孔和形貌退化。此前,研究者尝试替代掺杂剂或无掺杂空穴材料,但往往难以兼顾普适性和峰值性能。更务实的思路是:不替换Li⁺,而是通过分子螯合把它固定住。已有TCPO、EC、DES、吡啶/咪唑类添加剂等工作,但分子设计常受限于单一配位类别或配位位点不足,难以同时实现Li⁺完全固定和HTL性能优化。

 

分子设计:TPABT的“多位点螯合”

研究团队设计并合成了一系列D-A-D型小分子TPABT1、TPABT2、TPABT3。其苯并噻二唑单元上的N原子和甲氧基(–OMe)侧链可与Li⁺结合;随–OMe数量增加,TPABT3表现出最高的Li⁺结合能力和电子密度。DFT计算显示,TPABT3中Li⁺–Oᵒᵐᵉ结合能可达−3.52 eV,N–Li⁺–Oᵒᵐᵉ配位构型结合能达−3.61 eV,优于TPABT1/2。⁷Li和¹H NMR显示,TPABT3加入后Li⁺共振位移,TPABT3质子信号上移,说明N/O与Li⁺发生配位;固态NMR也证实该多配位构型在成膜后仍稳定存在。Mulliken电荷分析表明,Li⁺配位后TPABT3中Cᵒᵐᵉ电子密度增加。简言之,TPABT3像“多爪螯合剂”,通过N和–OMe氧共同抓住Li⁺,减少Li,TFSI聚集和LiₓOᵧ副产物。

抑制Li⁺迁移,促进p型掺杂TOF-SIMS深度剖析直观展示了效果:在85°C老化5天后,对照器件中Li⁺明显扩散至银电极和钙钛矿层;而TPABT3掺杂器件中Li⁺主要局限在HTL内,其他层信号很弱。TPABT3掺杂HTL中的Li⁺强度比对照高约两个数量级,说明Li⁺被有效固定。AFM显示,对照Spiro-OMeTAD薄膜老化后出现大量凹坑,源于Li-TFSI迁移和聚集;TPABT掺杂后凹坑明显减少,RMS粗糙度从9.64 nm降至TPABT3的7.67 nm。XPS中对照膜在56.1 eV出现强Li信号,而TPABT掺杂膜几乎消失,进一步证明Li⁺扩散被抑制。更妙的是,TPABT并非“旁观者”。EPR和UV-vis表明,TPABT不直接参与p型掺杂,而是通过螯合Li⁺促进TFSI⁻解离,提高TFSI⁻浓度,从而推动Spiro-OMeTAD氧化平衡正向移动,加速生成Spiro-OMeTAD⁺·TFSI⁻。无氧条件下则观察不到自由基信号,说明该过程依赖氧参与。结果,TPABT3掺杂膜空穴迁移率从1.73×10⁻³提升至1.97×10⁻³ cm² V⁻¹ s⁻¹,电导率从1.74×10⁻⁴提升至2.50×10⁻⁴ S cm⁻¹,载流子浓度从0.94×10⁹提升至2.5×10⁹ cm⁻³。

有序堆积与能级对齐GIWAXS显示,TPABT掺入后Spiro-OMeTAD在1.29 Å⁻¹处的π–π堆积峰增强,晶体相干长度从8.28 Å增至10.17 Å,说明分子堆积更有序、结晶性更好。原位吸收光谱显示,TPABT3使Spiro-OMeTAD结晶生长时间从0.804 s延长至1.165 s,为分子组织提供充足时间。UPS结果显示,TPABT3掺杂HTL的费米能级从−4.15 eV下移至−4.36 eV,价带顶从−5.17 eV移至−5.27 eV,与钙钛矿VBM(−5.38 eV)更匹配,有利于空穴提取和VOC提升。TRPL中,钙钛矿/TPABT3-HTL的载流子寿命从无HTL的1.27 μs降至332.49 ns,且PL淬灭更强,表明空穴提取加快,而非缺陷复合主导。

2.0.png

器件性能:26.03%器件结构为FTO/SnO₂/FAPbI₃/HTL/Ag,采用两步法制备FAPbI₃,TPABT最优掺杂浓度为5 mol%。结果:对照:PCE 23.85%,JSC 25.85 mA cm⁻²,VOC 1.16 V,FF 79.45%;TPABT1:PCE 24.79%;TPABT2:PCE 25.42%;TPABT3:PCE 26.03%,JSC 26.39 mA cm⁻²,VOC 1.17 V,FF 84.08%。迟滞指数从对照的2.3%降至TPABT3的0.4%,说明Li⁺迁移和界面电荷累积被有效抑制。EQE积分电流为25.91 mA cm⁻²,与J-V结果吻合;650–780 nm长波区EQE增强,归因于钙钛矿/HTL界面能级优化。20个器件统计也显示掺杂HTL重复性更好。

3.0.png
Photovoltaic performance and long-term stability of devices. (a) The device structure of PSCs. (b) Current density-voltage characteristics of the control and doped Spiro-OMeTAD champion devices. (c) EQE spectra and the integrated J sc. (d) PCE comparison between this work and reported high-efficiency two-step regular FAPbI3 PSCs. (e) Mott–Schottky plots of control and doped devices. (f) The TPC decay curves of control and doped devices. (g) Dark I-V curves of control and doped devices. (h) The device FF limitation composed of non-radiative loss and charge transport loss. (i) Storage stability of control and doped devices. (j) Operational stability of the unencapsulated control and doped devices at MPP under continuous 1 sun irradiation.

稳定性:1000 h后保持90%以上未封装TPABT3器件在ISOS-L-1条件(连续1 sun光照、MPP跟踪、氮气气氛、约40°C)下运行1000 h后,仍保持90%以上初始PCE;对照器件衰减明显。存储稳定性测试中,TPABT3器件在25±5°C、35±5%RH下1500 h也保持更优。稳定性提升来自多重协同:多齿螯合固定Li⁺、抑制Li-TFSI聚集和界面退化;TPABT促进Spiro-OMeTAD有序堆积和p型掺杂;能级对齐改善空穴提取,减少界面复合。

结论与意义该工作证明,多位点小分子螯合不是简单“加添加剂”,而是从配位化学层面重构Li-TFSI掺杂Spiro-OMeTAD体系:既保留Li⁺的掺杂功能,又抑制其迁移副作用,同时提升HTL形貌、堆积、电导和界面能级。TPABT3使n-i-p FAPbI₃电池效率达到26.03%,并在ISOS-L-1条件下实现1000 h保持90%以上的运行稳定性。该策略为高效、稳定n-i-p钙钛矿光伏的空穴传输层分子工程提供了可推广思路。

 

D-新new

武汉海山科技有限公司 

电话17720597715

027-86637880

OAMSA

辛胺甲基磺酸盐

1450981-06-2

>99%

BAMSA

丁胺甲基磺酸盐

53892-58-3

>99%

DAMSA

癸胺甲基磺酸盐


>99%

PEATFA

苯乙胺三氟醋酸盐

203525-17-1

>99%

p-F-PEATFA

对氟苯乙胺三氟醋酸盐


>99%

p-F-PMATFA

4-氟苯甲胺三氟醋酸盐


>99%

BATFA

丁胺三氟醋酸盐

24922-69-8

>99%

MATFA

甲胺三氟醋酸盐

107326-29-4

>99%

DPAc-TRZ

10-(4-(4,6-二苯基-1,3,5-三唑-2-基)苯基)-9,9-二苯基- 9,10-二氢吖啶



PF8Cz

聚(9,9-n-二辛基-2,7-芴-alt-9-异辛基-3,6-咔唑)





论文信息

Xinbao Lin, Xiangyang Zhang, Guanghao Meng, et al. Molecular Engineering of Multi-Site Small-Molecule Chelation for Highly Efficient and Stable n-i-p Perovskite Solar Cells. AdvancedScience, 2026. DOI: 10.1002/advs.78721.
转载内容(视频、文章、广告等)只以信息传播为目的,仅供参考,不代表本公众号认同其观点和立场也不作为投资意见及建议。内容的真实性、准确性和合法性由原作者负责。如涉及侵权,请联系删除,此转载不作为商业用途。


相关新闻资讯

钙钛矿电池的“长寿密码”:缺陷钝化不能只看初始效率

2026/11/18

钙钛矿电池的“长寿密码”:缺陷钝化不能只看初始效率——从陷阱抑制到稳定界面的五种机制钙钛矿太阳能电池效率进步惊人,但“缺陷容忍”不等于“缺陷免疫”。表面、晶界和埋底界面的缺陷,仍会带来非辐射复合、离子迁移、迟滞和长期衰减。Young Wook Noh 与 Jinsong Huang 在 Accounts of Materials Research 的 Account 文章中,把缺陷钝化从“补悬挂键

26.03%!多位点小分子“螯合”Li⁺,让n-i-p钙钛矿更高效、更稳定

2026/11/18

26.03%!多位点小分子“螯合”Li⁺,让n-i-p钙钛矿更高效、更稳定Li-TFSI掺杂的Spiro-OMeTAD是高效n-i-p钙钛矿太阳能电池的“标杆”空穴传输层,但Li⁺迁移长期被视为高性能与高稳定性之间的难解矛盾。近日,河北师范大学、大连理工大学、云南师范大学等合作团队在 Advanced Science 发表研究,提出多位点小分子螯合策略:设计D-A-D型分子TPABT1/2/3,利

突破26.88%!ACS Energy Lett:非离子酞菁添加剂实现钙钛矿电池“钝化+应变缓冲”双效合一

2026/11/17

突破26.88%!ACS Energy Lett:非离子酞菁添加剂实现钙钛矿电池“钝化+应变缓冲”双效合一在追求更高效率的同时,钙钛矿太阳能电池(PSCs)的长期运行稳定性始终是商业化道路上的“拦路虎”。如何在不引入额外移动离子的前提下,同时解决缺陷迁移、残余晶格应变和热机械降解这三大痛点?近期,南方科技大学/香港城市大学等团队在《ACS Energy Letters》上发表最新成果,提出了一种基