Melting point |
199-201 °C(lit.) |
Boiling point |
552.2±29.0 °C(Predicted) |
Density |
1.238±0.06 g/cm3(Predicted) |
solubility |
DMF: soluble |
form |
Solid |
pka |
4.77±0.10, most acidic, temperature: 25°C |
λmax |
341nm, 325nm (MeOH) |
Major Application |
Boron-doped diamond (BDD) substrates; Langmuir-Blodgett films; thin films; vacuum-deposited films |
Biological Applications |
Assessing role of membrane domains in lipid trafficking/sorting; characterizing interactions/mass transfer of surfactants inside crystaline protein matrixes; investigating transport/metabolism of cellular lipids; monitoring domain formation in membranes; implantable biocathodes/composite electrodes; nucleic acid hybridization probe; as a substrate for measuring cholesterylester hydrolase (CEH) activity, sphingosine kinases and activity |